Abstract
Mixtures of low-melting glasses (glazes) and barium hexaferrite magnetic powders sinter at relatively low temperatures (800° C) and produce dense items in which excessive grain growth has been inhibited.
Similar content being viewed by others
References
J. S. Reed andR. Fulrath,J. Amer. Ceram. Soc. 56 (1973) 207.
F. Kools,Ber. Dt. Keram. Ges. 55 (1978) 301.
F. Stäblein,ibid. 55 (1978) 305.
H. E. Shutz andH. W. Hennicke,ibid. 55 (1978) 308.
E. Lucchini, F. Ricciardiello andG. Slokar, “Influenza dell'ossido di calcio sulle caratteristiche degli esaferriti di bario e stronzio” Nota 1. Pubbl. N. 82 (Istituto di Chimica Applicata e Industriale, Università di Trieste, 1979).
R. H. Arendt,J. Appl. Phys. 44 (1973) 3300.
H. Wullkopf,Intern, J. Magn. 3 (1972) 179.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Lucchini, E., Meriani, S. & Slokar, G. Sintering of glass bonded ceramic barium hexaferrite magnetic powders. J Mater Sci 18, 1331–1334 (1983). https://doi.org/10.1007/BF01111950
Received:
Accepted:
Issue Date:
DOI: https://doi.org/10.1007/BF01111950